Why Mobile Phone Batteries do not last as long as an EV Battery
Car makers are extending the driving range of the electric vehicle to resemble a gasoline-powered car. This requires larger batteries that grow exponentially with the distance driven. Figure 1 illustrates the estimated driving ranges with different battery systems and hydrogen as a function of size.
Doubling battery size does not extend the driving range linearly and the vehicle becomes inefficient with increasing weight. Li-ion performs better than lead acid in energy density, but no battery meets hydrogen with a fuel cell, or fossil fuel feeding the traditional internal combustion engine (not shown). Extending the driving range with a larger tank is almost negligible compared to oversizing a battery. There is a threshold as to battery size and weight in a vehicle; going beyond a critical point has a negative return and efficiency suffers because of increased vehicle weight.
Figure 1: Battery size as a function of driving range.
Oversizing the battery does not expand the driving range linearly.
Note: 35MPa hydrogen tank refers to 5,000psi.
Source: International Journal of Hydrogen Energy, 34, 6005-6020 (2009)
Batteries have low calorific value compared to fossil fuel and it makes little sense to power a freight train, ocean-going ship or large airplane with batteries. A study reveals that replacing kerosene with batteries could keep an aircraft airborne for less than 10 minutes. Cost is another issue and batteries take long to charge. A fill-up that is quickly and conveniently as topping a tank with liquid or gaseous fuel is impossible with an electrochemical device. Charging also needs high power. An ultra-fast EV charge draws the equivalent electrical power of five households. Charging a fleet of EVs could dim a city.
Conversely, fossil fuel cannot match the qualities of a battery that is clean, quiet, and has an instant start-up with the flick of a switch. Although fossil fuel is cheap and readily available, frivolous burning of this resource must stop to save our planet. Finding alternatives that are environmentally friendly, economical and durable is a challenge; the battery fills this requirement only in part.
Advancements made in battery technology in the last 20 years are insufficient to replace fossil fuel. Pushing the boundaries of the battery reminds us of its many limitations, which include low energy density; long charging times, high cost and a short life before the packs quits, often without warning. Table 2 illustrates the energy densities of common fuels, including the battery.
| Fuel | Energy by mass (Wh/kg) |
|---|---|
| Hydrogen (350 bar) | 39,300 |
| Gasoline, diesel, natural gas (250 bar) | 12,000–13,000 |
| Body fat | 10,500 |
| Black coal (solid), Methanol | 6,000–7,000 |
| Wood (average) | 2,300 |
| Lithium-ion battery | 100–250 |
| Lead acid battery | 40 |
| Compressed air | 34 |
| Supercapacitor | 5 |
Table 2: Energy densities of fossil fuel and batteries.
Fossil fuel carries many times the energy per mass compared to batteries, but electrical power can be utilized more efficiently than burning fossil fuel.
Compiled from various sources. Values are approximate.
How to Prolong Battery Life
Driving range is a key consideration when buying an EV. Cost also plays a role but seldom is battery life mentioned. This may not be the concern for a tire-kicker, nor does the salesman want to alarm the buyer of possible service issues later on. What sells is the joy of electric propulsion that is clean, quiet and exhilarating. Taxpayer subsidies also help.
Batteries have a defined life span and this is apparent with the decreasing runtime in our mobile phones. EV advocates may argue that a smartphone battery cannot be compared to an EV battery; these products are totally different. That is true, but ironically both use lithium-ion systems. This article looks at the battery in an EV and mobile phone in terms of runtime and longevity.
The battery in the mobile phone is consumer grade, optimized for maximum runtime at low cost. the EV battery, on the other hand, is made to industry standards with longevity in mind. The dissimilarities do not stop there and a key difference is how the energy is dispensed.
A mobile phone gets charged at the end of a day and the stored energy can be fully utilized until the battery goes empty. In other words, the user has full access to the stored energy. When the battery is new, the phone provides good runtimes but this decreases with use. In this full cycle mode, Li-ion delivers about 500 cycles. The user adjusts to the decreasing runtime, and being a consumer product, the end of battery life often corresponds with a broken screen or the introduction of a new model. Built-in obsolescence serves well for device manufacturers and retailers.
The EV battery also ages and the capacity fades, but the EV manufacturer must guarantee the battery for eight years. This is done by oversizing the battery. When the battery is new, only about half of the available energy is utilized. This is done by charging the pack to only 80% instead of a full charge, and discharging to 30% when the available driving range is spent. As the battery fades, more of the battery storage is demanded. The driving range stays constant but unknown to the driver, the battery is gradually charged to a higher level and discharged deeper to compensate for the fade.
Once the battery capacity has dropped to 80%, the oversize protection is consumed and the battery maintenance system (BMS) applies a full charge and discharge. This exposes the EV battery to a similar stress level of a mobile phone and the driver begins noticing reduced driving range. Battery replacement may become necessary but the cost will be steep and higher than a combustion engine.
The EV begins to impersonate a mobile phone in terms of obsolescence when the battery fades. This may be the time when the buyer is flooded with faster and flashier models; something the smartphone user is all too familiar with, but price will be the shocker. It’s still too early to tell how long an EV battery will last. Some say the battery will outlive the car and find secondary application in energy storage systems.
Driving habits and temperature also affects aging, a characteristic that came to light when EV batteries operating in a warm climate faded prematurely. It was learned that keeping a battery at elevated temperature and high state-of-charge causes more stress than aggressive driving. In other words, keeping a fully charged Li-ion at 30°C (86°F) and above hastens the aging process more than driving at a moderate temperature. Many EV batteries include liquid cooling to reduce heat-related battery fade.
Harsh loading also reduces battery life. Because of its large size, the EV battery is only being stressed moderately, even during acceleration. In comparison, the mobile phone draws continuous high current from a small battery when transmitting and crunching data. This puts more stress on a mobile phone battery than driving an EV. A battery is also negatively impacted by the pulsed load of a mobile phone rather than the DC load of an EV. (See BU-501: Basic about Discharging.)
The EV does not disclose the battery capacity to the driver and only reveals state-of-charge (SoC) in the form of driving range. This is done in part for fear of customer complaints should the capacity drop below the mandated level at the end of the warranty period. Less knowledge is often better. The same restriction applies to a mobile phone battery, although access codes for service personnel are often available. A new battery has (should have) a capacity of 100%; 80% is the typical end of battery life.
Dynamic Stress Tests (DST) on Li-ion
All Li-ion batteries fade with time and use, whether in consumer products or enduring industrial use. Figure 3 explores the longevity of Li-ion batteries with different charge and discharge end points.
Figure 3: Capacity loss of Li-ion as a function of charge and discharge cut-off points.
Limiting a full charge and discharge prolongs battery life but lowers utilization.
Source: ResearchGate – Modeling of Lithium-Ion Battery Degradation for Cell Life Assessment. ResearchGate is a social networking site for scientists and researchers founded in 2008 to share papers, ask and answer questions, and to find collaborators. Wikipedia https://www.researchgate.net/publication/303890624_Modeling_of_Lithium-Ion_Battery_Degradation_for_Cell_Life_Assessment
The Li-ion batteries in the above table perform well but the largest capacity loss occurs with the pack that is charged to 100% and discharged to 25% (black stars). Cycling between 85% and 25% (green) provides longer service life than charging to 100% and discharging to 50% (dark blue).
The lowest capacity loss occurs when charging Li-ion to 75% and discharging to 65%. This, however, takes oversizing to the extreme and the battery is underutilized. Such practice is applied in satellites to achieve high cycle life and less for terrestrial applications as it increases cost, size and weight beyond a reasonable point of return. The dynamic stress test does not include a battery that is charged to 100% and discharged to zero, as is the case with a mobile phone. A full cycle provides the best battery utilization but reduces longevity.
Batteries tested in a laboratory do not always replicate true life conditions, and the results tend to be better than experienced in field use. In a lab environment, batteries are cycled over a period of a few months, often at controlled temperature and with an ideal charge and discharge regime. Random usage in real life adds the exposure to heat, vibration and harsh charging practices.
Summary
Batteries do not have a fixed life span, nor do they die suddenly but fade gradually. Environmental conditions, and not cycling alone, govern longevity. The user has some control to prolong battery life by avoiding ultra-fast charges, operating at moderate temperature and avoiding full charges. Avoiding harsh loads and full discharges also helps. Heat is the enemy of most batteries and the worst condition is keeping a fully charged Li-ion battery at elevated temperatures. Even with the best of care, a battery only lives for a season and the pack will eventually face retirement when power fades.
About the Author
Isidor Buchmann is the founder and CEO of Cadex Electronics Inc. For three decades, Buchmann has studied the behavior of rechargeable batteries in practical, everyday applications, has written award-winning articles including the best-selling book “Batteries in a Portable World,” now in its fourth edition. Cadex specializes in the design and manufacturing of battery chargers, analyzers and monitoring devices. For more information on batteries, visit www.batteryuniversity.com; product information is on www.cadex.com.
Last Updated: 27-Sep-2018
Batteries In A Portable World
The material on Battery University is based on the indispensable new 4th edition of "Batteries in a Portable World - A Handbook on Rechargeable Batteries for Non-Engineers" which is available for order through Amazon.com.
Find An Article
Table of Contents
-
Introduction 4>
- BU-001: Sharing Battery Knowledge
- BU-002: Introduction
- BU-003: Dedication
-
Crash Course on Batteries 4>
- BU-101: When Was the Battery Invented?
- BU-102: Early Innovators
- BU-103: Global Battery Markets
- BU-103a: Battery Breakthroughs: Myth or Fact?
- BU-104: Getting to Know the Battery
- BU-104a: Comparing the Battery with Other Power Sources
- BU-104b: Battery Building Blocks
- BU-104c: The Octagon Battery – What makes a Battery a Battery
- BU-105: Battery Definitions and what they mean
- BU-106: Advantages of Primary Batteries
- BU-106a: Choices of Primary Batteries
- BU-107: Comparison Table of Secondary Batteries
-
Battery Types 4>
- BU-201: How does the Lead Acid Battery Work?
- BU-201a: Absorbent Glass Mat (AGM)
- BU-201b: Gel Lead Acid Battery
- BU-202: New Lead Acid Systems
- BU-203: Nickel-based Batteries
- BU-204: How do Lithium Batteries Work?
- BU-205: Types of Lithium-ion
- BU-206: Lithium-polymer: Substance or Hype?
- BU-208: Cycling Performance
- BU-209: How does a Supercapacitor Work?
- BU-210: How does the Fuel Cell Work?
- BU-210a: Why does Sodium-sulfur need to be heated
- BU-210b: How does the Flow Battery Work?
- BU-211: Alternate Battery Systems
- BU-212: Future Batteries
- BU-214: Summary Table of Lead-based Batteries
- BU-215: Summary Table of Nickel-based Batteries
- BU-216: Summary Table of Lithium-based Batteries
- BU-217: Summary Table of Alternate Batteries
- BU-218: Summary Table of Future Batteries
-
Packaging and Safety 4>
- BU-301: A look at Old and New Battery Packaging
- BU-301a: Types of Battery Cells
- BU-302: Series and Parallel Battery Configurations
- BU-303: Confusion with Voltages
- BU-304: Why are Protection Circuits Needed?
- BU-304a: Safety Concerns with Li-ion
- BU-304b: Making Lithium-ion Safe
- BU-304c: Battery Safety in Public
- BU-305: Building a Lithium-ion Pack
- BU-306: What is the Function of the Separator?
- BU-307: How does Electrolyte Work?
- BU-308: Availability of Lithium
- BU-309: How does Graphite Work in Li-ion?
- BU-310: How does Cobalt Work in Li-ion?
- BU-311: Battery Raw Materials
-
Charge Methods 4>
- BU-401: How do Battery Chargers Work?
- BU-401a: Fast and Ultra-fast Chargers
- BU-402: What Is C-rate?
- BU-403: Charging Lead Acid
- BU-404: What is Equalizing Charge?
- BU-405: Charging with a Power Supply
- BU-406: Battery as a Buffer
- BU-407: Charging Nickel-cadmium
- BU-408: Charging Nickel-metal-hydride
- BU-409: Charging Lithium-ion
- BU-409a: Why do Old Li-ion Batteries Take Long to Charge?
- BU-409b: Charging Lithium Iron Phosphate
- BU-410: Charging at High and Low Temperatures
- BU-411: Charging from a USB Port
- BU-412: Charging without Wires
- BU-413: Charging with Solar, Turbine
- BU-413a: How to Store Renewable Energy in a Battery
- BU-414: How do Charger Chips Work?
- BU-415: How to Charge and When to Charge?
-
Discharge Methods 4>
- BU-501: Basics about Discharging
- BU-501a: Discharge Characteristics of Li-ion
- BU-502: Discharging at High and Low Temperatures
- BU-503: Determining Power Deliver by the Ragone Plot
- BU-504: How to Verify Sufficient Battery Capacity
-
"Smart" Battery 4>
- BU-601: How does a Smart Battery Work?
- BU-602: How does a Battery Fuel Gauge Work?
- BU-603: How to Calibrate a “Smart” Battery
- BU-603a: Calibrating SMBus Batteries with Impedance Tracking
- BU-604: How to Process Data from a “Smart” Battery
- BU-605: Testing and Calibrating Smart Batteries
-
From Birth to Retirement 4>
- BU-701: How to Prime Batteries
- BU-702: How to Store Batteries
- BU-703: Health Concerns with Batteries
- BU-704: How to Transport Batteries
- BU-704a: Shipping Lithium-based Batteries by Air
- BU-704b: CAUTION & Overpack Labels
- BU-704c: Class 9 Label
- BU-704d: NFPA 704 Rating
- BU-704e: Battery for Personal and Fleet Use
- BU-705: How to Recycle Batteries
- BU-705a: Battery Recycling as a Business
- BU-706: Summary of Do's and Don'ts
-
How To Prolong Battery Life 4>
-
General 4>
- BU-801: Setting Battery Performance Standards
- BU-801a: How to Rate Battery Runtime
- BU-801b: How to Define Battery Life
- BU-802: What Causes Capacity Loss?
- BU-802a: How does Rising Internal Resistance affect Performance?
- BU-802b: What does Elevated Self-discharge Do?
- BU-802c: How Low can a Battery be Discharged?
- BU-803: Can Batteries Be Restored?
- BU-803a: Cell Matching and Balancing
- BU-803b: What causes Cells to Short?
- BU-803c: Loss of Electrolyte
-
Lead Acid 4>
- BU-804: How to Prolong Lead-acid Batteries
- BU-804a: Corrosion, Shedding and Internal Short
- BU-804b: Sulfation and How to Prevent it
- BU-804c: Acid Stratification and Surface Charge
- BU-805: Additives to Boost Flooded Lead Acid
- BU-806: Tracking Battery Capacity and Resistance as part of Aging
- BU-806a: How Heat and Loading affect Battery Life
-
Nickel-based 4>
- BU-807: How to Restore Nickel-based Batteries
- BU-807a: Effect of Zapping
-
Lithium-ion 4>
- BU-808: How to Prolong Lithium-based Batteries
- BU-808a: How to Awaken a Sleeping Li-ion
- BU-808b: What Causes Li-ion to Die?
- BU-808c: Coulombic and Energy Efficiency with the Battery
- BU-809: How to Maximize Runtime
- BU-810: What Everyone Should Know About Aftermarket Batteries
- BU-811: Assuring Minimum Operational Reserve Energy (MORE)
-
Battery Testing and Monitoring 4>
- BU-901: Fundamentals in Battery Testing
- BU-901b: How to Measure the Remaining Useful Life of a Battery
- BU-902: How to Measure Internal Resistance
- BU-902a: How to Measure CCA
- BU-903: How to Measure State-of-charge
- BU-904: How to Measure Capacity
- BU-905: Testing Lead Acid Batteries
- BU-905a: Testing Starter Batteries in Vehicles
- BU-905b: Knowing when to Replace a Starter Battery
- BU-906: Testing Nickel-based Batteries
- BU-907: Testing Lithium-based Batteries
- BU-907a: Battery Rapid-test Methods
- BU-907b: Advancements in Battery Testing
- BU-907c: Cloud Analytics in Batteries
- BU-908: Battery Management System (BMS)
- BU-909: Battery Test Equipment
- BU-910: How to Repair a Battery Pack
- BU-911: How to Repair a Laptop Battery
- BU-915: Testing Battery with EIS
- BU-916: Deep Battery Diagnostics
- BU-917: In Search for Performance Transparency with Batteries
- BU-918: Battery Endurance Plan
- BU-919: Building a Matrix to test Batteries
- BU-920: Matrix Library
- BU-921: Testing Batteries by Multi-Model EIS
- BU-922: What Causes Starter Batteries to Fail?
- BU-923: Getting Deep Cycle Batteries Mission Ready
- BU-924: Battery Ecosystem
- BU-925: EIS Direct Drive, non-invasive Capacity Test
- BU-926: Battery Diagnostics, an Overlooked Requirement
-
Amazing Value of a Battery 4>
- BU-1001: Batteries in Industries
- BU-1002: Electric Powertrain, then and now
- BU-1002a: Hybrid Electric Vehicles and the Battery
- BU-1002b: Environmental Benefit of the Electric Powertrain
- BU-1003: Electric Vehicle (EV)
- BU-1003a: Battery Aging in an Electric Vehicle (EV)
- BU-1004: Charging an Electric Vehicle
- BU-1005: Does the Fuel Cell-powered Vehicle have a Future?
- BU-1006: Cost of Mobile and Renewable Power
- BU-1007: Net Calorific Value
- BU-1008: Working towards Sustainability
- BU-1009: Battery Paradox - Afterword
-
Information 4>
- BU-1101: Glossary
- BU-1102: Abbreviations
- BU-1103: Bibliography
- BU-1104: About the Author
- BU-1105: About Cadex (Sponsor)
- BU-1106: Author's Creed
- BU-1107: Disclaimer
- BU-1108: Copyright
-
Learning Tools 4>
- BU-1501 Battery History
- BU-1502 Basics about Batteries
- BU-1504 Battery Test and Analyzing Devices
- BU-1505 Short History of Cadex
-
Battery Articles 4>
- Perception of a Battery Tester
- Green Deal
- Risk Management in Batteries
- Predictive Test Methods for Starter Batteries
- Why Mobile Phone Batteries do not last as long as an EV Battery
- Battery Rapid-test Methods
- How to Charge Li-ion with a Parasitic Load
- Ultra-fast Charging
- Assuring Safety of Lithium-ion in the Workforce
- Diagnostic Battery Management
- Tweaking the Mobile Phone Battery
- Battery Test Methods
- Battery Testing and Safety
- How to Make Battery Performance Transparent
- Battery Diagnostics On-the-fly
- Making Battery State-of-health Transparent
- Batteries will eventually die, but when and how?
- Why does Pokémon Go rob so much Battery Power?
- How to Care for the Battery
- Tesla’s iPhone Moment — How the Powerwall will Change Global Energy Use
- Painting the Battery Green by giving it a Second Life
- Charging without Wires — A Solution or Laziness
- What everyone should know about Battery Chargers
- A Look at Cell Formats and how to Build a good Battery
- Battery Breakthroughs — Myth or Fact?
- Rapid-test Methods that No Longer Work
- Shipping Lithium-based Batteries by Air
- How to make Batteries more Reliable and Longer Lasting
- What causes Lithium-ion to die?
- Safety of Lithium-ion Batteries
- Recognizing Battery Capacity as the Missing Link
- Managing Batteries for Warehouse Logistics
- Caring for your Starter Battery
- Giving Batteries a Second Life
- How to Make Batteries in Medical Devices More Reliable
- Possible Solutions for the Battery Problem on the Boeing 787
- Impedance Spectroscopy Checks Battery Capacity in 15 Seconds
- How to Improve the Battery Fuel Gauge
- Examining Loading Characteristics on Primary and Secondary Batteries
-
Language Pool 4>
- BU-001: Compartir conocimiento sobre baterías
- BU-002: Introducción
- BU-003: Dedicatoria
- BU-104: Conociendo la Batería
- BU-302: Configuraciones de Baterías en Serie y Paralelo
-
Batteries in a Portable World book 4>
- Change-log of “Batteries in a Portable World,” 4th edition: Chapters 1 - 3
- Change-log of “Batteries in a Portable World,” 4th edition: Chapters 4 - 10