BU-1101: Glossary
AC: Alternating current; current flows in both directions. Household current is AC.
Acid: Compound in a battery that promotes electrochemical reaction.
AGM: Absorbent Glass Mat is a lead acid battery that uses a glass mat to promote the recombination of gases produced by the charging process.
Allotrope: Two or more forms of the same element in the same physical state (solid, liquid, gas) that differ from each other in physical and sometimes chemical properties.
Ampere-hours: Symbol Ah is a unit of charge. Example: Drawing a current of one ampere (1A) from a battery for one hour (1h) equates in one ampere-hour (1Ah).
Anode: Electrode on which oxidation occurs; releases electrons on discharge. When applying power to a device (vacuum tube, diode, battery on charge), the anode is positive; taking power away on discharge turns the anode to negative.
Antimony: Used in lead acid batteries to improve mechanical strengths of lead plates and enhances performance. Other uses are flame proofing, producing low friction applications, and building semiconductors.
ASoC: Absolute state-of-charge; ability to take specified charge when the battery is new.
ASoH: Absolute state-of-health; ability to store specified energy when the battery is new.
Barrel: Measuring unit for liquids (oil); 1 barrel has 42 US gallons, 35 Imperial gallons, 159 liters.
Basel Convention: International treaty to reduce the movements of hazardous waste between nations; signed in1989 in Basel, Switzerland and made effective in 1992.
Battery: Electrochemical cell, or cells, connected in series (some in parallel); composed of the anode (negative electrode), cathode (positive electrode), separator and electrolyte as catalyst.
Battery cycle: Charge followed by a discharge and recharge. No standard exists as to level of charge and discharge to constitute a cycle.
Battery Directive 2006/66/EC: European legislation on waste batteries to protect the environment.
BESS: Battery energy storage system (also known as ESS)
BMS: Battery Management System used inside or outside a battery to manage charge, discharge and provide SoC; forms an essential part to assure battery longevity and safety.
Bluetooth: Low-power radio communications up to 10 meters (30 feet). Bluetooth borrowed the name from Harald Bluetooth, a Danish king who lived more than 1,000 years ago.
Boolean bit: System of symbolic logic devised by George Boole in the 1840s; used in computers.
Button cell: Miniaturized battery also known as coin cell. Most are non-rechargeable.
Calcium: Fifth most abundant element by mass in the earth crust; essential for living organisms to build bone, teeth and shells. Discovered by Humphry Davy (1778–1829). Improves mechanical strength of lead plates in lead acid batteries; enhances performance.
Candela (cd): Unit of luminous intensity; agreed international name since 1967.
Capacitance: Unit measuring the electrical charge in a capacitor (condenser), measured in farad (f).
Capacitor: Component consisting of two conductive surfaces separated by an insulator. Passes AC; indefinite resistance for DC; voltage lags behind the current (opposite of a coil).
Capacity: Electrical energy of a battery in ampere-hours (Ah). The stored energy is measured by observing the elapsed time while discharging at a constant current to the end-of-discharge voltage. The capacity is the leading health indicator of a battery.
Capacity offset: Capacity correction when discharging a battery at a higher C-rate than specified.
Carbon dioxide: (CO2) Odorless gas formed during combustion, respiration and decomposition of organic substances. Plants absorb CO2; excess CO2 is blamed for climate change.
Cathode: Electrode in an electrochemical cell in which reduction takes place by absorbing electrons. During discharge, the cathode is positive; reverse on charge.
C-code: Abbreviation for configuration code. C-code is stored in a battery adapter and configures the analyzer to the correct battery settings (Cadex systems).
Cell mismatch: Cells in a battery pack that have unequal capacities, voltages or resistive values.
Cell reversal: Cell polarity reverses on a deep discharge at high load. Damages affected cell.
Charge: Replenishing electrical charge to a cell or battery.
Chemical battery: Behavior of the actual battery as opposed to monitoring peripheral activities.
Cobalt (Co): Hard, lustrous, gray metal; used in batteries, magnets, and high-strength alloys.
Co-generation: Utilization of heat and kinetic force. Heat drives steam turbines; kinetic force produces electricity through a generator; charges a battery on deceleration.
Coke: Derivative of coal from which most gases have been removed through heating.
Coulomb: Unit of electric charge. One coulomb (1C) equals one ampere-second (1As).
Coulombic efficiency, also called faradaic efficiency or current efficiency describes the charge efficiency by which electrons are transferred in a batteries.
C rate: Unit by which charge and discharge times are scaled. At 1C, the battery charges and discharges at a current that is at par with the marked Ah(See BU-402)
Current-limiting charger: Keeps current constant and allows voltage to fluctuate. (NiCd, NiMH chargers)
Cycle: Charge/discharge/charge. No standard exists as to what constitutes a cycle.
Cycle life: Number of cycles a battery can deliver. (End of-battery-life for portable devices is commonly set to 80%.)
Cylindrical cell: Positive and negative plates are rolled up and placed into a cylindrical container.
DC: Direct current; current flows in one direction. A battery delivers a DC current.
DC-to-DC converter: Converts DC to a higher or lower voltage potential.
Delta temperature over delta time (dT/dt): Senses rate of temperature increase over a given time rather than by measuring the absolute value; used for full charge detection of nickel-based battery(See BU-407)
Digital battery: Peripheral that monitors battery activity associated with the smart battery.
DIN, IEC: Capacity of a starter battery is measured with a 0.2C-rate (5h) discharge of a fully charged battery to 1.55V/cell or a 0.05 (20h) discharge to 1.75V/cell.
DoD: Depth of discharge; 100% is full discharge; 80% is commonly used for specification.
Double-layer capacitor: Electrostatic storage device utilizing the electrical double layer effect that is formed near the surface of the carbon electrode; also called supercapacitors or ultracapacitors.
Driving range: EVs display the allowable driving rang range rather than capacity. As the capacity fades, battery gets charged more and discharged deeper. The full capacity is hidden.
Dumb battery: Basic electrochemical battery with no electronic intelligence with which to communicate.
Electrochemical impedance spectroscopy (EIS), also known as impedance spectroscopy; method to test electrochemical characteristics of a battery; EIS injects AC signals at different frequencies and analyzes the response. (See BU-904)
Electrode: Conductor or plate in a cell in which an electrochemical reaction occurs.
Electrolyte: Non-metallic conductor of electricity (typically liquid) placed between positive and negative electrodes of a battery. Ion movement enables current flow.
Electrolyte oxidation (EO): Formation of a restrictive film on the Li-ion cathode if the voltage is kept above 4.10V/cell. The longer the battery stays in a high voltage, the more pronounced the degradation will be.
Energy: Work measures over time. Multiplying voltage x current x time = Watt-hours (Wh). Energy is also given in joules (J); 1,000 joules are 0.277Wh.
Energy Cell: Battery cell designed for maximum capacity. Power density may be compromised.
Energy density: Also known as volumetric energy density; specifies the amount of energy a cell can hold in volume (Wh/l). Energy density is synonymous with the runtime of a battery.
Energy Star: Organization promoting energy efficiency.
Exercise: In battery maintenance, one or several discharge cycles to the end-of-discharge with recharge; prevents memory buildup in NiCd and NiMH batteries.
Farad (f): Charge in coulombs necessary to change the potential between the plates of a capacitor by 1V. (1 Farad = 1 Coulomb per Volt)
Fast charge: 1–3 hours charge time.
Float charge: Similar to trickle or maintenance charge; compensates self-discharge of lead acid battery.
Flow battery: A cross between a conventional battery and a fuel cell. Liquid electrolyte of metallic salts is pumped through a core with positive and negative electrodes, separated by a membrane. The resulting ion exchange generates electricity. (See BU-210b)
Frequency: Number of events in a given time. Indicates how often the AC voltage changes from positive to negative per second, or how many times a battery is cycled.
Fuel cell: Device converts oxygen and hydrogen into electricity and water. (See BU-210)
Fuel gauge: State-of-charge (SoC) indicator to estimate the charge level of a battery.
Fuzzy logic: Multi-valued, mathematical logic derived from blurred data derives at a voted result. Battery rapid testing, image recognition, weather forecasting and medical tests follow fuzzy logic.
Graphene: Allotrope of carbon in a two-dimensional hexagonal lattice in which one atom forms each vertex; establishes the basic structural element of graphite, charcoal diamonds and more.
Graphite: A form of carbon with hexagonally crystallized allotrope, used in lead pencils, lubricants, batteries and the anode of most Li-ion.
Gravimetric energy density: Also known as specific energy; indicates the amount of energy a cell holds in weight (Wh/kg); synonymous with battery runtime.
Halon: Agent to suppress fire. Used also for Li-ion fires.
Hertz (Hz): Unit of frequency; 1Hz constitutes one full cycle per second.
Hydrogen (H): Chemical element with atomic number 1; lightest and most abundant chemical element; constitutes roughly 75% of the universe's elemental mass. Hydrogen gas becomes explosive at a concentration of 4 percent.
Hydrometer: Device to measure the specific gravity of a fluid; reads state-of-charge of a lead acid and other flooded batteries.
Hysteresis charge: Charger turns off at full charge and resumes after a time to compensate for parasitic loads and self-discharge.
I2C: Inter-Integrated Circuit is a multi-master, multi-slave, single-ended, serial computer bus invented by Philips Semiconductor.
IEC 60079: Intrinsically safe standards to prevent explosion in areas of flammable gas and dust.
IEC 60086: Safety standard for primary batteries.
IEC 62133: Safety requirements for sealed secondary cells/batteries for portable use.
IEEE 1625: Standard for rechargeable batteries for mobile computing devices.
IEEE 1725: Standard for rechargeable cells/batteries for mobile phones.
Imaginary impedance: Also known as complex impedance; characterizes the electrical resistance of reactive components as a function of frequency. Rising frequency lowers the capacitive resistance and increases the inductance resistance.
Impedance: Combination of capacitive, inductive and ohmic resistance; measured in ohms (R); frequency dependent.
Inductance (L): Winding that causes an electromotive force when current is applied; frequency dependent; reacts opposite to a capacitor; measurement in Henry (H.
Intelligent battery: Also known as smart battery; enables communication between device, charger and user.
Internal resistance: Electrical resistance of a battery pack in milliohms (m). A good battery has low resistance; corrosion raises it.
Intrinsically safe battery: Has built-in protection circuit to enable safe operation in a hazardous area; prevents sparks by limiting voltage and current spikes.
Ion: Atom or molecule with unequal number of electrons and protons; provides a positive or negative electrical charge.
Joule (J): Energy measurement: 1 joule = 1A at 1V for 1 second. Also applies to mechanical energy.
Lead acid battery: Oldest rechargeable battery; used as starter battery wheeled mobility, UPS, etc.
Lithium (Li): Soft, silver-white metal belonging to the alkali metal group; lightest and least dense metal in the element family; discovered by Johan August Arfwedson in 1817; metal is named after the Greek word “lithos” meaning “stone.”
Lithium battery: Has lithium-metal anode; most are non-rechargeable.
Lithium-ion battery: Rechargeable battery with cobalt, manganese, nickel and/or other metals as cathode and graphite anode.
Lithium-ion polymer battery: Similar to Li ion with a solid polymer as electrolyte; addition of gelled material promotes conductivity.
Lithium polymer battery: Also known as solid-state battery; uses solid polymer as electrolyte; heat induces conductivity.
Load current: Current flow when applying an electrical load.
Manchester coding, also known as phase coding, is used in 1-Wire battery communications to combine data and clock in a single-wire system
Manganese (Mn): Cathode material of Li-ion. Also used in steelmaking.
Matrix: Lookup table to compare and derive at characteristics, such as battery capacity.
Max Error: Expected margin of error (%) of charge calibration on SMBus battery.
Memory: Reversible capacity loss in nickel-based batteries.
Microsecond (μs): One-millionth of a second (10-6).
Milliampere-hour (mAh): Specifies battery capacity or rating; 1000mAh equals 1Ah.
Millihertz: Unit of frequency. Example: 1 Hertz = 1 cycle/second; 1mHz = 1,000 seconds.
Millisecond (ms): One-thousand of a second (10-3).
Nano: Latin for dwarf. 1 nanometer (nm) is one-billionth (10-9) of a meter or a layer of 3–6 atoms.
NCA: Nickel-cobalt-aluminum Li-ion; serves as cathode material.
Negative delta V (NDV): Drop in battery voltage when sealed NiCd and NiMH reach full charge; used to detect full charge.
Newton (N): Unit of force named after Isaac Newton; equal to accelerating 1kg a distance of 1 meter per second; (1N = 0.2248 pounds of force).
Nickel-cadmium battery (NiCd): Rechargeable battery using cadmium as anode and nickel as cathode.
Nickel-hydrogen battery (NiH): Rechargeable battery for satellites; pressure vessel contains the hydrogen.
Nickel-iron battery (NiFe): Rechargeable battery developed by Thomas Edison in 1901.Used for mining; powered German V-1 flying bomb and the V-2 rockets during World War II.
Nickel-metal-hydride battery (NiMH): Similar to NiCd; anode made of a hydride alloy that is less toxic than cadmium; 30 percent more capacity than NiCd but is less durable.
Nickel-zinc battery (NiZn): Similar to NiCd; first developed in 1920; short life due to dendrite growth.
Nit: Unit of brightness equal to one candela per square meter.
NMC: Lithium-ion with nickel, manganese and cobalt as cathode material.
Nominal voltage: Terminal voltage of batteries.
Nyquist plots: Invented by Harry Nyquist (1889–1976) while working at Bell Laboratories; provides the frequency response of a linear system that displays both amplitude and phase angle on a single plot using frequency as parameter.
Ohmic resistance: Electrical DC resistance with no capacitive and inductive reactance.
OhmTest™: Battery resistance measurement based on IEC 61951 (Cadex trademark).
Organic: Relating or belonging to carbon-based chemical compounds. Also relates to an organism, a living entity. Organic matter is the product of decay from a once living organism
Overcharge: Exceeding charge acceptance. The battery heats up, produces gases and is subject to an evet.
Overpack: Package can contain other non-dangerous or compatible dangerous good items. Limit is one package in accordance with Section II of PI 965. (Effective 1 April 2016).
Parasitic load: Power consumption with the device turned off.
Passivation layer: Resistive layer that forms on some batteries after prolonged storage. Applying a brief load breaks the layer and enables current flow.
Peukert law: Calculates battery capacity on discharge rate; higher rates decrease capacity. Mainly used for lead acid batteries; a reading close to 1 indicates a battery with minimal loss; larger number reflect higher losses; named after Wilhelm Peukert (1897).
Phosphate: Salt or phosphoric acid.
Polymer: Electrical insulator that passes ions.
Pouch cell: Packaged into a flexible, heat-sealable foil pouch similar to wrapping food products.
Power: Voltage x current = power in watts (W). Also in horsepower (1hp = 746W).
Power Cell: Battery cell designed for maximum current delivery. Energy density may be compromised.
Power density: Also known as volumetric power density; reflects loading capability of a battery.
Power factor: Ratio of real power versus apparent power. The unity power factor of 1 delivers 100% current to a load; a power factor of 0.50 reduces the contribution to 50%. A purely resistive load (heater elements) has a unity power factor of 1; a purely capacitive or inductive load has a power factor of 0.
Primary battery: Non-rechargeable battery.
Prismatic cell: A battery in which the positive and negative plates are stacked instead of rolled.
Protection circuit: Electronic circuit in a battery pack maintains safety when exceeding design limits.
Quick charger: Charges a battery in 3–6 hours.
QuickSort™: Classifies battery state-of-health into good, low and poor (Cadex trademark).
QuickTest™: Method to quick-test battery state-of-health (Cadex trademark).
Ragone chart: Plots battery performance on specific energy versus specific power
Randles Model: Equivalent electrical circuit representing electrolyte resistance in a battery that is commonly used in electrochemical impedance spectroscopy (EIS).
Rapid charge: Same as quick charge.
Reactance: Inductive and capacitive resistance; frequency dependent.
Recondition: Secondary discharge applied after end-of-discharge to drain the battery further; helps break down crystalline formation (memory) of nickel-based batteries(See BU-807)
Reformer: Device that extracts hydrogen from fossil and other fuels.
Reserve Capacity: American way of measuring battery capacity by applying a fixed discharge current and measuring time in minutes. Europe uses the ampere-hour (Ah) method under DIN and IEC. DIN and IEC mark the battery in Ah at a typical discharge of 0.2C-rate (5h-rate). See Abbreviation.
Residual capacity: Remaining battery capacity before charge.
Resistance: Restriction to current flow; high resistance generates voltage drop and heat.
Reverse load charge: Intersperses discharge pulses between charge pulses to promote the recombination of gases generated during fast charge; reduces memory.
RSoC: Relative state-of-charge; available charge with capacity fade (also known as SoC).
RSoH: Relative state-of-health; available storage capability when battery is broken in (also known as SoH)
Runtime: The length of time a battery provides power with a charge.
SAE J537: Test standard for 12V automotive starter batteries.
RC: Apply a full charge (charge to 14.4–16V at 16°C–43°C (60°F–110°F)). After a 24h rest, apply a regulated 25A discharge to 10.50V (1.75V/cell). Readings are in minutes of discharge time known as “Reserve Capacity” (RC).
CCA: Fully charge the battery and cool to -18°C (0°F) for 24 hours. While cold, apply a discharge current equal to the specified CCA reading. To pass, the voltage must stay above 7.2V (1.2V/cell) for 30 seconds.
SAE J1634: Test standard for electric vehicle; energy consumption, range.
SAE J1772: North American standard for electrical connectors for electric vehicles.
Secondary battery: Rechargeable battery
Self-discharge: Capacity loss due to internal leakage.
Separator: Isolates cathode and anode in a battery; acts as catalyst to promote ion movement from cathode to anode on charge and in reverse on discharge.
Siemens (s): Unit of electric conductance; equal to reciprocal ohm. Named after Ernst Werner von Siemens (1816–1892).
Silver-zinc: Rechargeable battery with high specific energy for defense and aerospace; has a short cycle life; is expensive.
Single-wire Bus: Simplified smart battery with one wire providing digital communications.
Slow charge: Overnight charge lasting 10–16 hours at a charge current of 0.1C.
Smart battery: Also known as an intelligent battery; communicates with device, charger and user.
SMBus: System Management Bus is a two-wire interface based on I2C; communicates with the battery and device by accepting control parameters and providing battery status, such as state-of-charge, manufacturer information, cycle count and error messages.
Sodium-nickel-chloride: Further development of sodium-sulfur battery. Zeolite Battery Research Africa Project (ZEBRA) made the battery commercially viable; must be heated for operation, used for large UPS and EVs.
Sodium–sulfur (NaS): Molten-salt battery; gained attention in 1970s, 1980s; has a short service life and high manufacturing costs; superseded by the sodium-nickel-chloride battery.
Soft cell: High cell resistance. The voltage drops on a load and is unable to clamp on charge. Very cold temperature and lack of electrolyte causes this condition.
Solid electrolyte interface (SEI): A film composed of lithium oxide and lithium carbonate forms on the surface of the Li-ion anode. The SEI layer grows with cycling and can form a barrier to obstruct ion flow.
Sol: Used by planetary astronomers to refer to the duration of a solar day on Mars. A Mars solar day has a mean period of 24 hours 39 minutes 35.244 seconds.
Specific energy: Also known as gravimetric energy density; indicates the amount of energy a cell contains in weight (Wh/kg); relates to battery capacity; governs runtime.
Specific gravity (SG): Weight ratio of a chemical solution compared to water at a specified temperature. SG of water is 1.0; the electrolyte of a fully charged lead acid battery is about 1.30.
Specific power: Also known as gravimetric power density; reflects the loading capability or the amount of current the battery can deliver; readings in W/kg.
Spectro™: Multi-model electrochemical impedance spectroscopy. Scans battery with a frequency and compares the signatures against matrices representing various conditions. (Cadex trademark) (See BU-904)
Spectroscopy: Analysis of a compound or a battery when scanned with a frequency.
Spinel: Hard glassy mineral consisting of an oxide of magnesium and aluminum that forms a three-dimensional chemical structure. Manganese-based Li ion has such a spinel structure.
State-of-charge (SoC): Indicates charge level of a battery; normally measured in percent. SoC has no relationship with capacity.
State-of-function (SoF): Reflects battery readiness that verifies capacity, current delivery, voltage, SoC, self-discharge and more; measured in %. (Capacity, current delivery and SoC are most basic.)
State-of-health (SoH): Reflects battery performance that verifies capacity, current delivery, voltage and self-discharge; measured in %. SoH excludes SoC.
Sulfation: Formation of lead sulfate crystal in a lead acid battery that inhibits current flow; storage at low state-of-charge causes this.
Supercapacitor: Electrochemical capacitor also known as an ultracapacitor or double-layer capacitor; specific energy is a fraction of Li-ion. Has high cycle life; offers good cold temperature performances.
System Management Bus (SMBus): Protocol for smart battery (See SMBus in Glossary).
Thermal runaway: Uncontrolled disintegration of a battery from the inside out; can be caused by cell defect, overcharging, excess heat and other abusive conditions.
Thermal voltage: A voltage created by the junction of dissimilar metals when a temperature difference exists between these junctions
Thermistor: Electrical resistor that changes resistance with temperature.
Titanate: Substance used for anode material of some lithium-based batteries.
Trickle charge: Also known as maintenance charge, compensates self-discharge of a battery.
UL 1642: Safety acceptance test for lithium-based batteries by Underwriters Laboratories. Other agencies are IEC 62133, IEEE 1625, IEEE 1725, BAJ (Japan), UN. In 2010, UL 1642 transitioned to IEC 62133, made fully effective on 1 May 2012.
UN 38.3: Safety norms for shipping battery products
Universal Serial Bus (USB): Bi-directional data port featuring a 5-volt supply and two data lines to accommodate auxiliary devices and to charge batteries.
Valve-regulated lead acid (VRLA): Maintenance-free lead acid battery recombines oxygen (positive plate) with hydrogen (negative plate) on charge; valve regulates pressure by release of excess gases. Repeated venting will lead to dry out.
Vinylene carbonate: Additive to improve performance of Li-ion cathode.
Voltage (V): Electric energy potential per unit charge. 1V = 1J/Coulomb. (1,000 joules = 0.277Wh).
Voltage delay: During prolonged storage, some battery systems develop a passivation layer. This results in a momentarily lower voltage until the film is dissipated through discharge.
Voltage limit: Battery thresholds on charge and discharge.
Voltage-limiting charger: Current is allowed to fluctuate in saturation mode while the voltage is capped (lead acid and Li ion charging).
Volumetric energy density: Also known as energy density; specifies energy storage in volume (Wh/l). (See Energy Density in this Glossary)
Watt (W): Unit of power; ampere (A) times volt (V) equals watts (W).
Watt-hour (Wh): Unit of electrical energy equivalent to a power consumption of one watt for one hour (One watt-hour = 3600 Joules). Multiplying a battery voltage (V) by the rated capacity (Ah) gives the battery energy in Wh. Example: 14.4V x 2.5 Ah = 36 Wh.
Wi-Fi: Wireless Internet connections; based on 2.4GHz 802.11b standard.
Zapping: Applying a momentary current pulse to a battery to evaporate a short.
Zinc-air: Generates electrical energy by an oxidation process of zinc and oxygen. Most zinc-air batteries are non-rechargeable, provide high specific energy but have poor load capabilities.
Last Updated: 26-Apr-2019
Batteries In A Portable World
The material on Battery University is based on the indispensable new 4th edition of "Batteries in a Portable World - A Handbook on Rechargeable Batteries for Non-Engineers" which is available for order through Amazon.com.
Find An Article
Table of Contents
-
Introduction 4>
- BU-001: Sharing Battery Knowledge
- BU-002: Introduction
- BU-003: Dedication
-
Crash Course on Batteries 4>
- BU-101: When Was the Battery Invented?
- BU-102: Early Innovators
- BU-103: Global Battery Markets
- BU-103a: Battery Breakthroughs: Myth or Fact?
- BU-104: Getting to Know the Battery
- BU-104a: Comparing the Battery with Other Power Sources
- BU-104b: Battery Building Blocks
- BU-104c: The Octagon Battery – What makes a Battery a Battery
- BU-105: Battery Definitions and what they mean
- BU-106: Advantages of Primary Batteries
- BU-106a: Choices of Primary Batteries
- BU-107: Comparison Table of Secondary Batteries
-
Battery Types 4>
- BU-201: How does the Lead Acid Battery Work?
- BU-201a: Absorbent Glass Mat (AGM)
- BU-201b: Gel Lead Acid Battery
- BU-202: New Lead Acid Systems
- BU-203: Nickel-based Batteries
- BU-204: How do Lithium Batteries Work?
- BU-205: Types of Lithium-ion
- BU-206: Lithium-polymer: Substance or Hype?
- BU-208: Cycling Performance
- BU-209: How does a Supercapacitor Work?
- BU-210: How does the Fuel Cell Work?
- BU-210a: Why does Sodium-sulfur need to be heated
- BU-210b: How does the Flow Battery Work?
- BU-211: Alternate Battery Systems
- BU-212: Future Batteries
- BU-214: Summary Table of Lead-based Batteries
- BU-215: Summary Table of Nickel-based Batteries
- BU-216: Summary Table of Lithium-based Batteries
- BU-217: Summary Table of Alternate Batteries
- BU-218: Summary Table of Future Batteries
-
Packaging and Safety 4>
- BU-301: A look at Old and New Battery Packaging
- BU-301a: Types of Battery Cells
- BU-302: Series and Parallel Battery Configurations
- BU-303: Confusion with Voltages
- BU-304: Why are Protection Circuits Needed?
- BU-304a: Safety Concerns with Li-ion
- BU-304b: Making Lithium-ion Safe
- BU-304c: Battery Safety in Public
- BU-305: Building a Lithium-ion Pack
- BU-306: What is the Function of the Separator?
- BU-307: How does Electrolyte Work?
- BU-308: Availability of Lithium
- BU-309: How does Graphite Work in Li-ion?
- BU-310: How does Cobalt Work in Li-ion?
- BU-311: Battery Raw Materials
-
Charge Methods 4>
- BU-401: How do Battery Chargers Work?
- BU-401a: Fast and Ultra-fast Chargers
- BU-402: What Is C-rate?
- BU-403: Charging Lead Acid
- BU-404: What is Equalizing Charge?
- BU-405: Charging with a Power Supply
- BU-406: Battery as a Buffer
- BU-407: Charging Nickel-cadmium
- BU-408: Charging Nickel-metal-hydride
- BU-409: Charging Lithium-ion
- BU-409a: Why do Old Li-ion Batteries Take Long to Charge?
- BU-409b: Charging Lithium Iron Phosphate
- BU-410: Charging at High and Low Temperatures
- BU-411: Charging from a USB Port
- BU-412: Charging without Wires
- BU-413: Charging with Solar, Turbine
- BU-413a: How to Store Renewable Energy in a Battery
- BU-414: How do Charger Chips Work?
- BU-415: How to Charge and When to Charge?
-
Discharge Methods 4>
- BU-501: Basics about Discharging
- BU-501a: Discharge Characteristics of Li-ion
- BU-502: Discharging at High and Low Temperatures
- BU-503: Determining Power Deliver by the Ragone Plot
- BU-504: How to Verify Sufficient Battery Capacity
-
"Smart" Battery 4>
- BU-601: How does a Smart Battery Work?
- BU-602: How does a Battery Fuel Gauge Work?
- BU-603: How to Calibrate a “Smart” Battery
- BU-603a: Calibrating SMBus Batteries with Impedance Tracking
- BU-604: How to Process Data from a “Smart” Battery
- BU-605: Testing and Calibrating Smart Batteries
-
From Birth to Retirement 4>
- BU-701: How to Prime Batteries
- BU-702: How to Store Batteries
- BU-703: Health Concerns with Batteries
- BU-704: How to Transport Batteries
- BU-704a: Shipping Lithium-based Batteries by Air
- BU-704b: CAUTION & Overpack Labels
- BU-704c: Class 9 Label
- BU-704d: NFPA 704 Rating
- BU-704e: Battery for Personal and Fleet Use
- BU-705: How to Recycle Batteries
- BU-705a: Battery Recycling as a Business
- BU-706: Summary of Do's and Don'ts
-
How To Prolong Battery Life 4>
-
General 4>
- BU-801: Setting Battery Performance Standards
- BU-801a: How to Rate Battery Runtime
- BU-801b: How to Define Battery Life
- BU-802: What Causes Capacity Loss?
- BU-802a: How does Rising Internal Resistance affect Performance?
- BU-802b: What does Elevated Self-discharge Do?
- BU-802c: How Low can a Battery be Discharged?
- BU-803: Can Batteries Be Restored?
- BU-803a: Cell Matching and Balancing
- BU-803b: What causes Cells to Short?
- BU-803c: Loss of Electrolyte
-
Lead Acid 4>
- BU-804: How to Prolong Lead-acid Batteries
- BU-804a: Corrosion, Shedding and Internal Short
- BU-804b: Sulfation and How to Prevent it
- BU-804c: Acid Stratification and Surface Charge
- BU-805: Additives to Boost Flooded Lead Acid
- BU-806: Tracking Battery Capacity and Resistance as part of Aging
- BU-806a: How Heat and Loading affect Battery Life
-
Nickel-based 4>
- BU-807: How to Restore Nickel-based Batteries
- BU-807a: Effect of Zapping
-
Lithium-ion 4>
- BU-808: How to Prolong Lithium-based Batteries
- BU-808a: How to Awaken a Sleeping Li-ion
- BU-808b: What Causes Li-ion to Die?
- BU-808c: Coulombic and Energy Efficiency with the Battery
- BU-809: How to Maximize Runtime
- BU-810: What Everyone Should Know About Aftermarket Batteries
- BU-811: Assuring Minimum Operational Reserve Energy (MORE)
-
Battery Testing and Monitoring 4>
- BU-901: Fundamentals in Battery Testing
- BU-901b: How to Measure the Remaining Useful Life of a Battery
- BU-902: How to Measure Internal Resistance
- BU-902a: How to Measure CCA
- BU-903: How to Measure State-of-charge
- BU-904: How to Measure Capacity
- BU-905: Testing Lead Acid Batteries
- BU-905a: Testing Starter Batteries in Vehicles
- BU-905b: Knowing when to Replace a Starter Battery
- BU-906: Testing Nickel-based Batteries
- BU-907: Testing Lithium-based Batteries
- BU-907a: Battery Rapid-test Methods
- BU-907b: Advancements in Battery Testing
- BU-907c: Cloud Analytics in Batteries
- BU-908: Battery Management System (BMS)
- BU-909: Battery Test Equipment
- BU-910: How to Repair a Battery Pack
- BU-911: How to Repair a Laptop Battery
- BU-915: Testing Battery with EIS
- BU-916: Deep Battery Diagnostics
- BU-917: In Search for Performance Transparency with Batteries
- BU-918: Battery Endurance Plan
- BU-919: Building a Matrix to test Batteries
- BU-920: Matrix Library
- BU-921: Testing Batteries by Multi-Model EIS
- BU-922: What Causes Starter Batteries to Fail?
- BU-923: Getting Deep Cycle Batteries Mission Ready
- BU-924: Battery Ecosystem
- BU-925: EIS Direct Drive, non-invasive Capacity Test
- BU-926: Battery Diagnostics, an Overlooked Requirement
-
Amazing Value of a Battery 4>
- BU-1001: Batteries in Industries
- BU-1002: Electric Powertrain, then and now
- BU-1002a: Hybrid Electric Vehicles and the Battery
- BU-1002b: Environmental Benefit of the Electric Powertrain
- BU-1003: Electric Vehicle (EV)
- BU-1003a: Battery Aging in an Electric Vehicle (EV)
- BU-1004: Charging an Electric Vehicle
- BU-1005: Does the Fuel Cell-powered Vehicle have a Future?
- BU-1006: Cost of Mobile and Renewable Power
- BU-1007: Net Calorific Value
- BU-1008: Working towards Sustainability
- BU-1009: Battery Paradox - Afterword
-
Information 4>
- BU-1101: Glossary
- BU-1102: Abbreviations
- BU-1103: Bibliography
- BU-1104: About the Author
- BU-1105: About Cadex (Sponsor)
- BU-1106: Author's Creed
- BU-1107: Disclaimer
- BU-1108: Copyright
-
Learning Tools 4>
- BU-1501 Battery History
- BU-1502 Basics about Batteries
- BU-1504 Battery Test and Analyzing Devices
- BU-1505 Short History of Cadex
-
Battery Articles 4>
- Perception of a Battery Tester
- Green Deal
- Risk Management in Batteries
- Predictive Test Methods for Starter Batteries
- Why Mobile Phone Batteries do not last as long as an EV Battery
- Battery Rapid-test Methods
- How to Charge Li-ion with a Parasitic Load
- Ultra-fast Charging
- Assuring Safety of Lithium-ion in the Workforce
- Diagnostic Battery Management
- Tweaking the Mobile Phone Battery
- Battery Test Methods
- Battery Testing and Safety
- How to Make Battery Performance Transparent
- Battery Diagnostics On-the-fly
- Making Battery State-of-health Transparent
- Batteries will eventually die, but when and how?
- Why does Pokémon Go rob so much Battery Power?
- How to Care for the Battery
- Tesla’s iPhone Moment — How the Powerwall will Change Global Energy Use
- Painting the Battery Green by giving it a Second Life
- Charging without Wires — A Solution or Laziness
- What everyone should know about Battery Chargers
- A Look at Cell Formats and how to Build a good Battery
- Battery Breakthroughs — Myth or Fact?
- Rapid-test Methods that No Longer Work
- Shipping Lithium-based Batteries by Air
- How to make Batteries more Reliable and Longer Lasting
- What causes Lithium-ion to die?
- Safety of Lithium-ion Batteries
- Recognizing Battery Capacity as the Missing Link
- Managing Batteries for Warehouse Logistics
- Caring for your Starter Battery
- Giving Batteries a Second Life
- How to Make Batteries in Medical Devices More Reliable
- Possible Solutions for the Battery Problem on the Boeing 787
- Impedance Spectroscopy Checks Battery Capacity in 15 Seconds
- How to Improve the Battery Fuel Gauge
- Examining Loading Characteristics on Primary and Secondary Batteries
-
Language Pool 4>
- BU-001: Compartir conocimiento sobre baterías
- BU-002: Introducción
- BU-003: Dedicatoria
- BU-104: Conociendo la Batería
- BU-302: Configuraciones de Baterías en Serie y Paralelo
-
Batteries in a Portable World book 4>
- Change-log of “Batteries in a Portable World,” 4th edition: Chapters 1 - 3
- Change-log of “Batteries in a Portable World,” 4th edition: Chapters 4 - 10