BU-908: Battery Management System (BMS)
Mercedes CEO Dieter Zetsche says, "The intelligence of the battery does not lie in the cell but in the complex battery system." This is reminiscent to computers in the 1970s that had big hardware but little software [1]
The purpose of a BMS is to:
Provide battery safety and longevity, a must-have for Li-ion.
Reveal state-of-function in the form of state-of-charge and state-of-health (capacity)
Prompt caution and service. This could be high temperature, cell imbalance or calibration.
Indicate end-of-life when the capacity falls below the user-set target threshold.
Not all BMS offer all these features. The most basic functions are battery protection and showing state-of-charge (SoC).
While SoC is helpful, the readout is incomplete without also tracking the capacity as the battery fades. The user may be accustomed to a battery that delivers full capacity, but this condition is temporary and cannot be maintained. Capacity is the primary indicator of battery state-of-health (SoH) and should be part of the battery management system (BMS). Knowing SoC and SoH provides state-of-function (SoF), the ultimate confidence of readiness, but technology to provide this information in an effective way is being improved.
Building a better BMS is a challenge when considering that we still lack a dependable method to read state-of-charge, the most basic measure of a battery(See BU-903: How to Measure State-of-charge) Reading the remaining energy in a battery is more complex than dispensing liquid fuel. While a fuel tank has a fixed dimension and delivers fuel which can be measured with great accuracy, an electrochemical storage system reduces its size and the in- and out-flowing coulombs cannot be assessed with great accuracy as the battery ages.
The BMS also provides protection when charging and discharging; it disconnects the battery if set limits are exceeded or if a failure occurs. Established BMS standards are the SMBus (System Management Bus) used for mostly portable applications, as well as the CAN Bus (Controller Area Network) and the simpler LIN Bus (Local Interconnect Network) for automotive use.
Stationary batteries were among the first to include supervisory systems and the most basic is voltage monitoring of individual cells. Some systems also include cell temperature and current measurement. Recording a slight difference in cell temperature hints to a problem, and measuring the voltage drop of each cell at a given load reveals cell resistance. Dry-out, corrosion, plate separation, and other malfunctions can thus be identified.
Although the BMS is effective in detecting anomalies; capacity fade, the most predictable health indicator, is difficult to estimate because voltage and internal resistance are commonly not affected. The ability to read capacity fade from 100 to 70 percent would be valuable, but most BMS cannot do this effectively and the battery might be given a clean bill of health even if the capacity has dropped to 50 percent. Most BMS only respond to anomalies that lie outside capacity estimation, such as voltage differences among cells caused by cell imbalances and a change in internal resistance.
Some industrial and medical device manufacturers use a date stamp to determine the end of battery life, others observe the cycle count. While counting cycles may be simplistic, no convention exists that defines a cycle and some systems simply call it a cycle when the battery is charged(See BU-501: Basics About Discharging) Date-stamping has similar shortcomings in that it promotes premature replacement of batteries that are seldom used, while the heavy hitters may stay in service too long(See BU-803: Can Batteries be Restored?) To reduce risk of failure, authorities mandate early replacement, and a two-year service life is common. Prolonged storage will give the batteries a very short working life.
Biomedical engineers are aware that most batteries are replaced too soon. iPhone owners have complained that their smartphones show 100 percent charge when the battery is only 90 percent charged. Even military leaders say that their battery arsenal for combat is so poor that many soldiers carry rocks instead of batteries. Effective battery management is either missing or is inadequate. Over-expectations with BMS are common and the user is stunned when stranded without battery power.
Let’s look at how a BMS works, note the shortcomings and examine up-and-coming technologies that could change the way batteries are monitored.
A BMS takes the imprint of the “chemical battery” during charging and discharge and establishes the “digital battery” that communicates with the user. Figure 1 illustrates the battery components consisting of stored energy, the empty portion that can be refilled and the inactive part that is permanently lost. Rated capacity refers to the manufacturer’s specified capacity in Ah (ampere-hours) that is only valid when the battery is new; available capacity designates the true energy storage capability derived by deducting the inactive part. State-of-charge (SoC) refers to the stored energy, which also includes the inactive part.
Figure 1: Three parts of a battery
A battery consists of stored energy, the empty portion that can be recharged and the inactive portion that is permanently lost due to aging.
A BMS is programmed to a rated capacity and it measures the in-and-outflowing coulombs that relate to the available capacity. As the capacity drops, the coulomb count decreases and this discrepancy enables capacity estimation. The most accurate readings are possible when counting the coulombs from a fully discharged battery during a complete charge or discharging a fully charged battery to the cut-off point. Such clean starts are seldom possible and real-life capacity estimations get muddled over time.
A BMS sets flags when receiving a full discharge and charge. During a rest period, an advanced BMS may also calculate SoC on hand of the stable open circuit voltage and begin counting the coulombs during charge and discharge from that vantage point. Some BMS also look at voltage recovery after removing a load to estimate SoC and/or SoH.
Battery Sensing by Voltage-Current-Temperature
The old Volkswagen Beetle had minimal battery problems. Its battery management system applied charge to the battery and burned the over-charge energy on a resistor while cruising through a relay-operated regulator. The car had no parasitic loads when parked.
Since then, modern vehicles have been inundated with onboard electronics to enhance safety, convenience, comfort and pleasure; features no one knew were needed. For the accessories to function reliably, the state-of-charge of the battery must be known at all times. This is especially critical with start-stop technology that is being adopted worldwide.
When the engine of a start-stop car is off at a red light, the battery draws 25–50 amperes to feed the lights, ventilators, windshield wipers and other accessories. The battery must have enough charge to crank the engine, which requires an additional 350A for a brief moment. When the engine runs again and the car accelerates to the posted speed limit, the battery only begins charging after a 10-second delay, a deferral allows channeling all energy to vehicle acceleration. When back in charge mode, the lead acid battery is notoriously slow in charging.
To provide vital battery information, luxury cars are fitted with a battery sensor that measure voltage, current and temperature. Figure 2 illustrates the electronic battery monitor (EBM) packaged in a small housing forming part of the positive battery clamp.
Figure 2: Battery sensor for starter battery
The sensor reads voltage, current and temperature to estimate state-of-charge and detect anomalies; capacity assessment is not possible.
The EBM works well when the battery is new but most sensors do not adjust correctly to aging. The SoC accuracy of a new battery is about +/–10 percent. With aging, the EBM begins to drift and the accuracy can drop to 20 percent and higher. This is in part connected to capacity fade, a value most BMS cannot estimate effectively. It is not an oversight by engineers; they fully understand the complexities and shortcomings involved.
A typical start-stop vehicle goes through about 2,000 micro cycles per year. Such a strain would reduce the capacity of a standard starter battery to about 60 percent and carmakers use different battery systems that include AGM and the Advanced Lead-carbon(Also see BU-806a: How Heat and Loading affect Battery Life)
Automakers want to ensure that no driver gets stranded in traffic with a dead battery. To conserve energy, modern cars turn off unnecessary accessories when the battery is low on charge and the motor stays on at a stoplight. Even with this measure, the state-of-charge can remain low if commuting in gridlock traffic because an idling motor does not provide much charge to the battery. With lights, windshield wipers and electric heating elements engaged there could be a net discharge.
Battery monitoring is also important on hybrid vehicles to optimize charge levels. Intelligent charge management prevents overcharge and avoids deep discharge. When the charge level is low, the internal combustion engine (ICE) engages earlier than normal and is left running longer for additional charge. On a fully charged battery the ICE turns off and the car moves on electric energy in slow traffic.
An EV driver expects similar accuracies in energy reserve as is possible with a fuel-powered vehicle but current technology does not allow this. To compensate, the EV battery is overrated and the fuel gauge is adjusted to preserve extra energy when the charge drops low to cover for inaccuracies. The EV driver is advised not to let the charge go too low but to charge more often. A mid-charger range is best for the battery.
The EV driver also anticipates the same driving range as the car ages. This is not possible and the drivable distance gets shorter with each passing year, but the BMS makes allowances. A new battery may only charge to about 80 percent and discharge to 30 percent. As the capacity fades, the bandwidth gradually increases, providing similar driving ranges as a new battery would. The distances traveled will be noticeably shorter when driving in cold temperatures because of reduced battery performance and once the battery has aged beyond the energy compensation band of the BMS(See BU-1003: Electric Vehicle)
Adding Capacity Estimation in BMS
The EBM has limitations in that it cannot estimate capacity effectively. This can be overcome by adding capacity estimations(See BU-904: How to Measure Capacity) Figure 3 shows a BMS with common sensing points to which the ability to measure capacity has been added. Spectro™ stands for electrochemical impedance spectroscopy (EIS) with complex modeling. This converts a simple battery sensor to the state-of-function (SoF) level.
Figure 3: Spectro-BMS™
adds capacity as key element to estimate battery state-of-health.
Knowing SoF improves battery validation, but some device manufacturers refuse to reveal capacity readings to a consumer that are less than 100 percent, especially during the warranty period. To conceal unwanted information, the data can be made code-accessible for service personnel use only(See also BU-602: How does a Battery Fuel Gauge Work?)
Consumer concerns put aside, SoF signifies a momentous improvement to BMS in terms of battery reliability as it tracks capacity fade and calculates the true runtime on the available energy. Capacity-based BMS will also predict eventual replacement, an issue that cannot be fully satisfied with current BMS technologies. Future BMS will combine the information of the “digital battery” with that of the “chemical battery” to provide reliable SoF data through advanced learn algorithms.
References
[1] Source: CleanTechnica
Last Updated: 4-Nov-2021
Batteries In A Portable World
The material on Battery University is based on the indispensable new 4th edition of "Batteries in a Portable World - A Handbook on Rechargeable Batteries for Non-Engineers" which is available for order through Amazon.com.
Find An Article
Table of Contents
-
Introduction 4>
- BU-001: Sharing Battery Knowledge
- BU-002: Introduction
- BU-003: Dedication
-
Crash Course on Batteries 4>
- BU-101: When Was the Battery Invented?
- BU-102: Early Innovators
- BU-103: Global Battery Markets
- BU-103a: Battery Breakthroughs: Myth or Fact?
- BU-104: Getting to Know the Battery
- BU-104a: Comparing the Battery with Other Power Sources
- BU-104b: Battery Building Blocks
- BU-104c: The Octagon Battery – What makes a Battery a Battery
- BU-105: Battery Definitions and what they mean
- BU-106: Advantages of Primary Batteries
- BU-106a: Choices of Primary Batteries
- BU-107: Comparison Table of Secondary Batteries
-
Battery Types 4>
- BU-201: How does the Lead Acid Battery Work?
- BU-201a: Absorbent Glass Mat (AGM)
- BU-201b: Gel Lead Acid Battery
- BU-202: New Lead Acid Systems
- BU-203: Nickel-based Batteries
- BU-204: How do Lithium Batteries Work?
- BU-205: Types of Lithium-ion
- BU-206: Lithium-polymer: Substance or Hype?
- BU-208: Cycling Performance
- BU-209: How does a Supercapacitor Work?
- BU-210: How does the Fuel Cell Work?
- BU-210a: Why does Sodium-sulfur need to be heated
- BU-210b: How does the Flow Battery Work?
- BU-211: Alternate Battery Systems
- BU-212: Future Batteries
- BU-214: Summary Table of Lead-based Batteries
- BU-215: Summary Table of Nickel-based Batteries
- BU-216: Summary Table of Lithium-based Batteries
- BU-217: Summary Table of Alternate Batteries
- BU-218: Summary Table of Future Batteries
-
Packaging and Safety 4>
- BU-301: A look at Old and New Battery Packaging
- BU-301a: Types of Battery Cells
- BU-302: Series and Parallel Battery Configurations
- BU-303: Confusion with Voltages
- BU-304: Why are Protection Circuits Needed?
- BU-304a: Safety Concerns with Li-ion
- BU-304b: Making Lithium-ion Safe
- BU-304c: Battery Safety in Public
- BU-305: Building a Lithium-ion Pack
- BU-306: What is the Function of the Separator?
- BU-307: How does Electrolyte Work?
- BU-308: Availability of Lithium
- BU-309: How does Graphite Work in Li-ion?
- BU-310: How does Cobalt Work in Li-ion?
- BU-311: Battery Raw Materials
-
Charge Methods 4>
- BU-401: How do Battery Chargers Work?
- BU-401a: Fast and Ultra-fast Chargers
- BU-402: What Is C-rate?
- BU-403: Charging Lead Acid
- BU-404: What is Equalizing Charge?
- BU-405: Charging with a Power Supply
- BU-406: Battery as a Buffer
- BU-407: Charging Nickel-cadmium
- BU-408: Charging Nickel-metal-hydride
- BU-409: Charging Lithium-ion
- BU-409a: Why do Old Li-ion Batteries Take Long to Charge?
- BU-409b: Charging Lithium Iron Phosphate
- BU-410: Charging at High and Low Temperatures
- BU-411: Charging from a USB Port
- BU-412: Charging without Wires
- BU-413: Charging with Solar, Turbine
- BU-413a: How to Store Renewable Energy in a Battery
- BU-414: How do Charger Chips Work?
- BU-415: How to Charge and When to Charge?
-
Discharge Methods 4>
- BU-501: Basics about Discharging
- BU-501a: Discharge Characteristics of Li-ion
- BU-502: Discharging at High and Low Temperatures
- BU-503: Determining Power Deliver by the Ragone Plot
- BU-504: How to Verify Sufficient Battery Capacity
-
"Smart" Battery 4>
- BU-601: How does a Smart Battery Work?
- BU-602: How does a Battery Fuel Gauge Work?
- BU-603: How to Calibrate a “Smart” Battery
- BU-603a: Calibrating SMBus Batteries with Impedance Tracking
- BU-604: How to Process Data from a “Smart” Battery
- BU-605: Testing and Calibrating Smart Batteries
-
From Birth to Retirement 4>
- BU-701: How to Prime Batteries
- BU-702: How to Store Batteries
- BU-703: Health Concerns with Batteries
- BU-704: How to Transport Batteries
- BU-704a: Shipping Lithium-based Batteries by Air
- BU-704b: CAUTION & Overpack Labels
- BU-704c: Class 9 Label
- BU-704d: NFPA 704 Rating
- BU-704e: Battery for Personal and Fleet Use
- BU-705: How to Recycle Batteries
- BU-705a: Battery Recycling as a Business
- BU-706: Summary of Do's and Don'ts
-
How To Prolong Battery Life 4>
-
General 4>
- BU-801: Setting Battery Performance Standards
- BU-801a: How to Rate Battery Runtime
- BU-801b: How to Define Battery Life
- BU-802: What Causes Capacity Loss?
- BU-802a: How does Rising Internal Resistance affect Performance?
- BU-802b: What does Elevated Self-discharge Do?
- BU-802c: How Low can a Battery be Discharged?
- BU-803: Can Batteries Be Restored?
- BU-803a: Cell Matching and Balancing
- BU-803b: What causes Cells to Short?
- BU-803c: Loss of Electrolyte
-
Lead Acid 4>
- BU-804: How to Prolong Lead-acid Batteries
- BU-804a: Corrosion, Shedding and Internal Short
- BU-804b: Sulfation and How to Prevent it
- BU-804c: Acid Stratification and Surface Charge
- BU-805: Additives to Boost Flooded Lead Acid
- BU-806: Tracking Battery Capacity and Resistance as part of Aging
- BU-806a: How Heat and Loading affect Battery Life
-
Nickel-based 4>
- BU-807: How to Restore Nickel-based Batteries
- BU-807a: Effect of Zapping
-
Lithium-ion 4>
- BU-808: How to Prolong Lithium-based Batteries
- BU-808a: How to Awaken a Sleeping Li-ion
- BU-808b: What Causes Li-ion to Die?
- BU-808c: Coulombic and Energy Efficiency with the Battery
- BU-809: How to Maximize Runtime
- BU-810: What Everyone Should Know About Aftermarket Batteries
- BU-811: Assuring Minimum Operational Reserve Energy (MORE)
-
Battery Testing and Monitoring 4>
- BU-901: Fundamentals in Battery Testing
- BU-901b: How to Measure the Remaining Useful Life of a Battery
- BU-902: How to Measure Internal Resistance
- BU-902a: How to Measure CCA
- BU-903: How to Measure State-of-charge
- BU-904: How to Measure Capacity
- BU-905: Testing Lead Acid Batteries
- BU-905a: Testing Starter Batteries in Vehicles
- BU-905b: Knowing when to Replace a Starter Battery
- BU-906: Testing Nickel-based Batteries
- BU-907: Testing Lithium-based Batteries
- BU-907a: Battery Rapid-test Methods
- BU-907b: Advancements in Battery Testing
- BU-907c: Cloud Analytics in Batteries
- BU-908: Battery Management System (BMS)
- BU-909: Battery Test Equipment
- BU-910: How to Repair a Battery Pack
- BU-911: How to Repair a Laptop Battery
- BU-915: Testing Battery with EIS
- BU-916: Deep Battery Diagnostics
- BU-917: In Search for Performance Transparency with Batteries
- BU-918: Battery Endurance Plan
- BU-919: Building a Matrix to test Batteries
- BU-920: Matrix Library
- BU-921: Testing Batteries by Multi-Model EIS
- BU-922: What Causes Starter Batteries to Fail?
- BU-923: Getting Deep Cycle Batteries Mission Ready
- BU-924: Battery Ecosystem
-
Amazing Value of a Battery 4>
- BU-1001: Batteries in Industries
- BU-1002: Electric Powertrain, then and now
- BU-1002a: Hybrid Electric Vehicles and the Battery
- BU-1002b: Environmental Benefit of the Electric Powertrain
- BU-1003: Electric Vehicle (EV)
- BU-1003a: Battery Aging in an Electric Vehicle (EV)
- BU-1004: Charging an Electric Vehicle
- BU-1005: Does the Fuel Cell-powered Vehicle have a Future?
- BU-1006: Cost of Mobile and Renewable Power
- BU-1007: Net Calorific Value
- BU-1008: Working towards Sustainability
- BU-1009: Battery Paradox - Afterword
-
Information 4>
- BU-1101: Glossary
- BU-1102: Abbreviations
- BU-1103: Bibliography
- BU-1104: About the Author
- BU-1105: About Cadex (Sponsor)
- BU-1106: Author's Creed
- BU-1107: Disclaimer
- BU-1108: Copyright
-
Learning Tools 4>
- BU-1501 Battery History
- BU-1502 Basics about Batteries
- BU-1504 Battery Test and Analyzing Devices
- BU-1505 Short History of Cadex
-
Battery Articles 4>
- Perception of a Battery Tester
- Green Deal
- Risk Management in Batteries
- Predictive Test Methods for Starter Batteries
- Why Mobile Phone Batteries do not last as long as an EV Battery
- Battery Rapid-test Methods
- How to Charge Li-ion with a Parasitic Load
- Ultra-fast Charging
- Assuring Safety of Lithium-ion in the Workforce
- Diagnostic Battery Management
- Tweaking the Mobile Phone Battery
- Battery Test Methods
- Battery Testing and Safety
- How to Make Battery Performance Transparent
- Battery Diagnostics On-the-fly
- Making Battery State-of-health Transparent
- Batteries will eventually die, but when and how?
- Why does Pokémon Go rob so much Battery Power?
- How to Care for the Battery
- Tesla’s iPhone Moment — How the Powerwall will Change Global Energy Use
- Painting the Battery Green by giving it a Second Life
- Charging without Wires — A Solution or Laziness
- What everyone should know about Battery Chargers
- A Look at Cell Formats and how to Build a good Battery
- Battery Breakthroughs — Myth or Fact?
- Rapid-test Methods that No Longer Work
- Shipping Lithium-based Batteries by Air
- How to make Batteries more Reliable and Longer Lasting
- What causes Lithium-ion to die?
- Safety of Lithium-ion Batteries
- Recognizing Battery Capacity as the Missing Link
- Managing Batteries for Warehouse Logistics
- Caring for your Starter Battery
- Giving Batteries a Second Life
- How to Make Batteries in Medical Devices More Reliable
- Possible Solutions for the Battery Problem on the Boeing 787
- Impedance Spectroscopy Checks Battery Capacity in 15 Seconds
- How to Improve the Battery Fuel Gauge
- Examining Loading Characteristics on Primary and Secondary Batteries
-
Language Pool 4>
- BU-001: Compartir conocimiento sobre baterías
- BU-002: Introducción
- BU-003: Dedicatoria
- BU-104: Conociendo la Batería
- BU-302: Configuraciones de Baterías en Serie y Paralelo
-
Batteries in a Portable World book 4>
- Change-log of “Batteries in a Portable World,” 4th edition: Chapters 1 - 3
- Change-log of “Batteries in a Portable World,” 4th edition: Chapters 4 - 10